IPC-4101E covers the requirements for base materials that are referred to as laminate or prepreg and listed in the specification sheets that are contained in the last of the main body. These are to be used primarily for rigid and multilayer printed boards for electronic interconnections. This document contains 65 individual specification sheets that can be searched using keywords. These keywords...
IPC JEDEC J-STD-020 is used to determine what moisture-sensitivity-level (MSL) classification level should be used so that surface mount devices (SMDs) can be properly packaged, stored and handled to avoid subsequent thermal and mechanical damage during the assembly solder reflow attachment and/or repair operation. J-STD-020 covers components to be processed at higher temperatures for lead-free...
The sole industry standard for determining appropriate internal and external conductor sizes on printed boards as a function of the current carrying capacity required and the acceptable conductor temperature rise. This document provides guidance on how thermal conductivity, vias, copper planes, power dissipation and printed board material and thickness all factor into the relationship between...
IPC-9191 reflects the principals of statistical process control (SPC) represented by ISO/DIS 11462-1, Guidelines for Implementation of Statistical Process Control (SPC) -- Part 1: Elements of SPC. This document outlines the SPC philosophy, implementation strategies, tools, and techniques used for relating process control and capability to final product requirements. Supersedes IPC-PC-90.
IPC-6012E specification covers qualification and performance of rigid printed boards, including single-sided, double-sided, with or without plated-through holes, multilayer with or without blind/buried vias and metal core boards. It addresses final finish and surface plating coating requirements, conductors, holes/vias, frequency of acceptance testing and quality conformance as well as electrical...
This specification establishes the general requirements and responsibilities for suppliers and users of printed boards. Serving as the foundation for the IPC-6010 Board Performance Documents series, it describes quality and reliability assurance requirements that must be met. For use with IPC-6012 through IPC-6018. Supersedes IPC-RB-276, IPC-SC-320, IPC-TC-500, IPC-ML-950C. 15 pages. Released July...
The industry's first specification for the evaluation of a legend and/or marking ink material for the determination of acceptability of use in a standard printed board system. IPC-4781 provides coverage for adhesion, material qualification and testing, resistances to solvents, requirements for resistance to lead-free solders, and electrical requirements. 17 pages. Released May 2008.
Contains over 150 industry approved test techniques and procedures for chemical, mechanical, electrical, and environmental tests on all forms of printed boards and connectors. New and updated test methods are available for download at https://www.ipc.org/test-methods.
Covers the various conductive and dielectric materials that can be used for the fabrication of HDI and microvias. The 23 specification sheets included in IPC/JPCA-4104 cover the qualification and conformance requirements for such materials as photoimageable dielectric dry films and liquids, epoxy blends and coated foils. IPC/JPCA-4104 also includes six new test methods developed specifically for...
Contains backplane design information from the fabrication and assembly perspective. Includes sections on design and documentation; fabrication; assembly; repair; and inspection. 17 pages. Revised September 1982.
The definitive standard on printed board dimensioning and tolerancing is finally here! IPC-2615 comprehensively covers dimensioning and tolerancing of electronic packaging and is consistent with other IPC printed board standards such as IPC-6012A and IPC-2221A. The document includes fundamental dimensioning and tolerancing rules, positional, profile, orientation and form tolerances and detailed...
Covers the materials, qualification, certification and performance requirements for multilayer polymer thick film (PTF) printed, extrusion deposited, or otherwise applied conductor, insulator and through-hole technology. This specification may also be used for procurement of single and double-sided boards. 59 pages. Released November 1989.
IPC-2316 offers printed board users and designers the necessary information for incorporating formed and placed embedded passive components into their applications. The history of embedded passive technologies is given along with full coverage of embedded resistors, capacitors and inductors. In addition, it also assists the user in understanding some of the physical, electrical and thermal...
The IPC-2228 standard establishes the specific requirements for the design of rigid, flexible and rigid-flexible printed boards utilizing radio frequency (RF) and/or Microwave circuity and/or high frequency laminates where RF transmission lines and related passive metal layers are considered as distributed circuits, instead of conventional lumped circuit elements. The IPC-2228 standard is used to...
Used in conjunction with IPC-2221A, IPC-2225 establishes the requirements and other considerations (thermal, electrical, electromechanical and mechanical) for the design of Single Chip Module (SCM-L), MCM or MCM-L assemblies. Key concepts include adhesive interconnection information, typical die attach materials, microvia material properties and relationships with DFM and DFE. 44 pages. Released...
The Joint Industry Guide Material Composition Declaration for Electrotechnical Products has been updated to include the most recent substances for restriction. The JIG-101 is an industry materials declaration guide that facilitates reporting of material content information across the global electrotechnical supply chain. This document sets minimum requirements for a materials declaration. The...
Covers requirements and test methods for thermally conductive dielectric adhesives used to bond components in place. Permanent, removable and self-shimming adhesives are addressed. 18 pages. Released January 1995.
Printed board quality encompasses many parameters, cleanliness being one important parameter. This document defines the recommended general requirements for the cleanliness of unpopulated (bare) single, double-sided and multilayer printed boards. Coverage is given to Ion Chromatography (IC) testing and Ionic cleanliness testing for process control. 6 pages. Released December 2009.
Establishes the specific requirements for organic mounting structures used to interconnect chip components, which in combination form the completed functional organic single-chip module (SCM-L) or organic multichip module (MCM-L) assembly. Includes the quality and reliability assurance requirements that must be met for their acquisition. For use with IPC-6011. 25 pages. Released February 1998.
This document describes materials that can be used for the fabrication of embedded passive resistor devices within the finished printed circuit board substrate. It provides information on general designations and associated characteristics of embedded passive device (EPD) resistor materials. The document shall be used as a qualification and conformance standard for designers and users when...
This standard establishes the requirements for the documentation of electronic diagrams used as the foundation for defining the electrical interconnectivity of electronic products. The description pertains to either schematic diagrams, logic diagrams or Boolean truth tables and includes methodology for defining circuit flow, electrical or functional restrictions, or maintenance test procedures...
IPC-4413 standard covers finished fabrics woven from low Dk electrical grade glass fiber yarns that are intended as a reinforcing material in laminated plastics for electrical and electronic use. All fabrics covered by IPC-4413 standard are plain weave.
Establishes design concepts, guidelines and procedures for reliable printed wiring assemblies. Focuses on SMT or mixed technology PWAs, specifically addressing the interconnect structure and the solder joint itself. Discusses substrates, components, attachment materials, coatings and assembly processes and testing considerations. In addition, this document contains detailed appendices covering...
This voluntary standard establishes minimum requirements for the design, installation, operation and maintenance of electrically heated process equipment in order to minimize electrical hazards and prevent fires that may occur in combustible tanks, tank liners and drying equipment.
This document describes a PWB fabrication data quality rating system used by fabricators to evaluate incoming data package integrity. Includes information on conformance to both fabricator and customer design rules and can be used by printed board designers as an output quality check. 16 pages. Released February 1999.
Coming Soon
IPC-7095E: Design and Assembly Process Implementation for Ball Grid Arrays (BGAs)
IPC-7530B: Guidelines for Temperature Profiling for Mass Soldering Processes (Reflow & Wave)
IPC-2294: Design Standard for Printed Electronics on Rigid Substrates
IPC-6904: Qualification and Performance Specifications for Printed Electronics on Rigid Substrates
IPC-4105: Specification for Metal Base Copper Clad laminates for Rigid Printed Boards