IPC-T-50N document is designed to provide definitions for terms commonly used in the electronics industry. The definitions are intended to provide sufficient clarity of detail such that a reader utilizing English as a second language could understand the subtleties of the meaning. IPC-T-50N contains over 550 new or revised terms, including new terminology for via structures, surface mount device...
IPC-6012F, covers qualification and performance of rigid printed boards, including single-sided, double-sided, with or without plated-through holes, multilayer with or without blind/buried vias and metal core boards. It addresses final finish and surface plating coating requirements, conductors, holes/vias, frequency of acceptance testing and quality conformance as well as electrical, mechanical...
IPC-6013E standard covers qualification and performance requirements for flexible printed boards designed to IPC-2221 and IPC-2223. The flexible printed board may be single-sided, double-sided, multilayer or rigid-flex multilayer. All of these constructions may include stiffeners, PTHs, microvias, and blind/buried vias. The IPC-6013E standard incorporates new and updated requirements for final...
IPC/JEDEC J-STD-033D provides surface mount device manufacturers and users with standardized methods for handling, packing, shipping and use of moisture/reflow sensitive components. These methods help avoid damage from moisture absorption and exposure to solder reflow temperatures that can result in yield and reliability degradation and damaged components. IPC/JEDEC J-STD-033D procedures provide a...
IPC/JEDEC J-STD-020F standard is to identify the classification level of nonhermetic SMDs designed for surface mount assembly that are sensitive to moisture-induced stress so that they can be properly packaged, stored, and handled to avoid damage during assembly solder reflow attachment and/or repair operations. IPC/JEDEC J-STD-020F standard may be used to determine what classification level...
The IPC-6018D standard covers qualification and performance of high frequency (microwave) boards, including single-sided, double-sided, with or without plated-through holes, multilayer with or without blind/buried vias and metal core boards. It addresses final finish and surface plating coating requirements, conductors, holes/vias, frequency of acceptance testing and quality conformance as well as...
IPC-4562A standard covers metal unsupported foils and foils supported by carrier films suitable for subsequent use in printed boards. IPC-4562B addresses the requirements of metal foils used in printed wiring applications.
IPC-4103B standard covers the requirements for clad and unclad plastic laminate and bonding layer materials to be used for the fabrication of printed boards for microstrip, stripline and high speed digital electrical and electronic circuits. In addition to better definitions of inclusions and how to properly classify them; redefine "substrates" as, "fabricated sheets"; and a more proper definition...
The IPC-4412C covers the requirements for reinforcements woven from "E"glass yarn. These reinforcements are used in the production of prepregs, some of which are pressed into laminates. These prepregs and laminates are the base materials for rigid and mulitlayer printed boards. The IPC-4412C standard contains tables which describe each fabriic style in detail including the yarn used, the number of...
IPC-9252 defines levels of appropriate testing and assists in the selection of the test analyzer, test parameters, test data and fixturing required to perform electrical test(s) on unpopulated printed boards and innerlayers. Revision B provides new requirements for resistive and indirect continuity and isolating testing, test record marking and traceability and an updated sample electrical test...
The IPC-7093A standard provides essential design and assembly guidance for implementing bottom termination components (BTCs). Specifically, IPC-7093A provides guidelines on critical design, materials, assembly, inspection, repair, quality, and reliability issues associated with BTCs.
The IPC-1921A handbook provides problems, causes and possible corrective actions related to printed board manufacturing processes. Includes more than 200 photos and illustrations depicting common defects.
The IPC-4202C standard covers the requirements for flexible base materials, herein referred to as laminates, prepregs or films, to be used primarily for flexible printed boards for electrical and electronic circuits
IPC/JEDEC J-STD-035A test method defines the procedures for performing acoustic microscopy on nonhermetic encapsulated electronic devices. IPC/JEDEC J-STD-035A method provides users with an acoustic microscopy process flow for detecting anomalies (delaminations, cracks, mold compound voids, etc.) nondestructively in encapsulated electronic devices while achieving reproducibility
This document includes lead free, no-clean, and environmental friendly chemistries. This is a collection of information on electronic board and assembly cleaning in a single location. This major revision explains the relationship between materials, processes, and contaminants in fabrication and assembly operations. It also addresses cleanliness assessment and process control in relation to...
IPC-2231A provides guidelines for establishing a best practice methodology for use in developing a formal DFX (Design for Manufacturing, Fabrication, Assembly, Testability, Cost, Reliability, Environment, Reuse) process for layout of printed boards.
The IPC-6017A standard defines the electrical, mechanical, and environmental requirements specific to embedded passive and active circuitry in printed boards. These requirements are in addition to the applicable requirements of other performance specification(s) (e.g., J-STD-001).
IPC-4203B establishes the classification system, the qualification and quality conformance requirements for dielectric films coated with an adhesive on one or both sides, which are to be used as cover material and/or bondply for flexible printed circuitry, as well as supported or unsupported adhesive films to be used in the fabrication of flexible printed circuitry. IPC-4203B does not cover non...
This guideline describes flexibility and stretchability testing to evaluate printable electronics for stretchable and wearable applications. 26 pages. Released March 2017
This document describes the design and assembly challenges and ways to address those challenges for implementing 3D component technology. Recognizing the effects of combining multiple uncased semiconductor die elements in a single-package format can impact individual component characteristics and can dictate suitable assembly methodology. The information contained in this standard focuses on...
This specification establishes the certification requirements for facilities that inspect/test printed boards, components and materials. This specification is intended to provide a minimum standardized basis for evaluating or auditing a technically oriented inspection/testing facility. Revised November 1997. 15 pages.
IPC-1730A is a tool used to categorize a laminate manufacturer's capabilities, which furnishes customer access to detailed information. Used for single or multiple sites or locations, IPC-1730A simplifies auditing processes and reduces the frequency of audits, decreasing paperwork and improving efficiency. The program includes a description, approval and certification profile and a quality profile...
IPC-7094A describes the design and assembly challenges for implementing flip chip technology in a direct chip attach (DCA) assembly. The effect of bare-die or die-size components in a flip chip format has an impact on component characteristics and dictates the appropriate assembly methodology. The IPC-7094A standard focuses on design, assembly methodology, critical inspection, repair and...
Surface Insulation Resistance (SIR) testing is a tool used not only for characterization testing of production processes such as solder masks, soldering flux, and conformal coatings, but also for examining the electrochemical reactions at each stage of the electronic assembly production process. This handbook covers the terminology, theories, test procedures and test vehicles of SIR testing...
This standard provides a marking and labeling system that aids in assembly, rework, repair and recycling and provides for the identification of: those assemblies that are assembled with lead-containing or lead-free solder; components that have lead-containing or lead-free second level interconnect terminal finishes and materials; the maximum component temperature not to be exceeded during assembly...
Coming Soon
IPC-7095E: Design and Assembly Process Implementation for Ball Grid Arrays (BGAs)
IPC-7530B: Guidelines for Temperature Profiling for Mass Soldering Processes (Reflow & Wave)
IPC-2294: Design Standard for Printed Electronics on Rigid Substrates
IPC-6904: Qualification and Performance Specifications for Printed Electronics on Rigid Substrates
IPC-4105: Specification for Metal Base Copper Clad laminates for Rigid Printed Boards