While there are a variety of industry test vehicles for the examination of material compatibility, the IPC-B-52 test board was created to meet the needs for testing both ion chromatograph and surface insulation resistance (SIR) which would be more representative of the manufacturing materials and processes. IPC-9203A standard addresses the IPC-B-52 test vehicle, which can be used to evaluate a...
The IPC-4202C standard covers the requirements for flexible base materials, herein referred to as laminates, prepregs or films, to be used primarily for flexible printed boards for electrical and electronic circuits
IPC-4103B standard covers the requirements for clad and unclad plastic laminate and bonding layer materials to be used for the fabrication of printed boards for microstrip, stripline and high speed digital electrical and electronic circuits. In addition to better definitions of inclusions and how to properly classify them; redefine "substrates" as, "fabricated sheets"; and a more proper definition...
IPC-4203B establishes the classification system, the qualification and quality conformance requirements for dielectric films coated with an adhesive on one or both sides, which are to be used as cover material and/or bondply for flexible printed circuitry, as well as supported or unsupported adhesive films to be used in the fabrication of flexible printed circuitry. IPC-4203B does not cover non...
IPC/JEDEC J-STD-035A test method defines the procedures for performing acoustic microscopy on nonhermetic encapsulated electronic devices. IPC/JEDEC J-STD-035A method provides users with an acoustic microscopy process flow for detecting anomalies (delaminations, cracks, mold compound voids, etc.) nondestructively in encapsulated electronic devices while achieving reproducibility
The IPC-9701B standard establishes a thermal cycling test method to characterize the fatigue lifetimes of surface mount solder attachments of electronic assemblies. The surface mount devices may be solder-attached to rigid, flexible or rigid-flex printed boards. The characterization results can be used to predict the field lifetime of solder attachments for the use environments and conditions of...
The IPC-1401A standard specifies the requirements and best practice guidelines for an effective corporate social responsibility (CSR) management system to help an enterprise integrate CSR as a customer requirement into products and value chain activities, as well as to identify and manage CSR risks and opportunities through cooperation with customers and suppliers, to enhance the competitive...
Provides requirements for dielectric adhesives to hold components in place from the mounting to the soldering process and identifies test methods to ensure their long term properties. 9 pages. Released December 2014.
IPC-2231A provides guidelines for establishing a best practice methodology for use in developing a formal DFX (Design for Manufacturing, Fabrication, Assembly, Testability, Cost, Reliability, Environment, Reuse) process for layout of printed boards.
This document is the product of the IPC Electrochemical Migration (ECM) Task Group. It was drafted to provide guidance regarding implementation of the User Guide for the IPC-TM-650, Method 2.6.25, Conductive Anodic Filament (CAF) Resistance and Other Internal Electrochemical Migration Testing to evaluate the effects of mechanical stress, laminate material fracturing, ionic contamination, moisture...
The IPC-6017A standard defines the electrical, mechanical, and environmental requirements specific to embedded passive and active circuitry in printed boards. These requirements are in addition to the applicable requirements of other performance specification(s) (e.g., J-STD-001).
IPC-7526A handbook addresses understencil cleanliness during stencil printing, removal of solder paste from stencils following the cleaning process and misprint PCB board cleaning considerations.
This standard provides and defines key characteristics and test methods for procuring printed electronics substrates. Includes six materials specification sheets.
The IPC-4412C covers the requirements for reinforcements woven from "E"glass yarn. These reinforcements are used in the production of prepregs, some of which are pressed into laminates. These prepregs and laminates are the base materials for rigid and mulitlayer printed boards. The IPC-4412C standard contains tables which describe each fabriic style in detail including the yarn used, the number of...
This guideline describes flexibility and stretchability testing to evaluate printable electronics for stretchable and wearable applications. 26 pages. Released March 2017
The IPC-9202A, Material and Process Characterization/Qualification Test Protocol that records changes in Surface Insulation Resistance (SIR) on a representative sample of a printed circuit assembly (PCA). It quantifies any deleterious effects that might arise from solder flux or other process residues left on external surfaces after soldering, which can cause unwanted electro-chemical reactions...
This document describes the design and assembly challenges and ways to address those challenges for implementing 3D component technology. Recognizing the effects of combining multiple uncased semiconductor die elements in a single-package format can impact individual component characteristics and can dictate suitable assembly methodology. The information contained in this standard focuses on...
The IPC-6903A standard provides 62 additional terms and definitions for the design and manufacture of printed electronics. The IPC-6903A standard creates a common language and understanding for the worldwide printed electronics community.
The IPC-4591A standard establishes the classification system and the qualification and quality conformance requirements for functional conductive materials used in printed electronics applications. It provides companies that procure functional materials for printed electronics with the necessary technical structure to design and manufacture products meeting conformance to industry-determined...
This specification sets requirements based on performance criteria for the use of Immersion Silver (IAg) as a surface finish for printed circuit boards. It is intended for use by chemical suppliers, printed board manufacturers, electronics manufacturing services (EMS) companies and original equipment manufacturers (OEM). IAg is a thin immersion deposit over copper. It is a multifunctional surface...
Strain gage testing allows for objective analysis of the strain and strain rate levels to which a surface mount package may be subjected to during assembly, test and operation. Excessive strain can result in various failure modes for different solder alloys, package types, surface finishes or laminate materials. This document describes specific guidelines for strain gage testing during the printed...
This specification establishes the certification requirements for facilities that inspect/test printed boards, components and materials. This specification is intended to provide a minimum standardized basis for evaluating or auditing a technically oriented inspection/testing facility. Revised November 1997. 15 pages.
IPC-1730A is a tool used to categorize a laminate manufacturer's capabilities, which furnishes customer access to detailed information. Used for single or multiple sites or locations, IPC-1730A simplifies auditing processes and reduces the frequency of audits, decreasing paperwork and improving efficiency. The program includes a description, approval and certification profile and a quality profile...
IPC-7094A describes the design and assembly challenges for implementing flip chip technology in a direct chip attach (DCA) assembly. The effect of bare-die or die-size components in a flip chip format has an impact on component characteristics and dictates the appropriate assembly methodology. The IPC-7094A standard focuses on design, assembly methodology, critical inspection, repair and...
Surface Insulation Resistance (SIR) testing is a tool used not only for characterization testing of production processes such as solder masks, soldering flux, and conformal coatings, but also for examining the electrochemical reactions at each stage of the electronic assembly production process. This handbook covers the terminology, theories, test procedures and test vehicles of SIR testing...